NITRIC ACID LEACHING OF NICKEL FROM SPENT GIAP-8 CATALYST: PRE-CALCINATION, RSM-BASED PROCESS OPTIMISATION AND KINETICS

Article Information

Download PDF

Abstract

This paper investigates the nitric acid leaching of nickel from spent
GIAP-8 catalyst used in the steam methane reforming stage of ammonia production.
The pre-calcination temperature (300–600 °C) was optimised to remove the coke
layer. The effects of HNO₃ concentration, temperature, liquid-to-solid (L:S) ratio,
time and particle size were evaluated by one-factor-at-a-time experiments and a
four-factor Box–Behnken design (response surface methodology, RSM). Under
optimal conditions (calcination at 450 °C; 3 M HNO3, 80 °C, L:S = 5:1, 4 h, < 0.5
mm) nickel recovery reached 97.3 ± 1.2 %. The second-order regression model
showed high adequacy (R² = 0.9818; predicted R² = 0.9134). Kinetic data were best
described by the chemical-reaction-controlled form of the shrinking core model.
Comparison with H2SO4 demonstrated the advantage of HNO3 in terms of recovery
and ease of downstream product processing.

Keywords

spent catalyst, GIAP-8, nickel, nitric acid, leaching, NiAl2O4 spinel, calcination, Box–Behnken design, shrinking core model.